Multi-Response Optimization of Dry Turning Parameters for Incoloy 800H Superalloy Using a Grey-Fuzzy Algorithm
Angappan Palanisamy, Duraiswamy Palanisamy, Abhishek Agarwal, Chellamuthu Prakash, Sembian Manoharan, Natarajan ManikandanIncoloy 800H (Fe–Ni–Cr) is an iron-based superalloy that is difficult to machine because of its rapid work-hardening behaviour. Although Taguchi-based grey relational analysis has previously been applied to machining optimisation problems, studies employing an integrated grey-fuzzy framework for the dry turning of Incoloy 800H remain limited. Therefore, the present investigation aims to develop and validate a grey-fuzzy optimisation approach for determining the optimal dry turning parameters of Incoloy 800H by simultaneously minimising machining forces, surface roughness, and specific cutting pressure. Cutting speed (35, 45, and 55 m/min), feed rate (0.02, 0.04, and 0.06 mm/rev), and depth of cut (0.5, 0.75, and 1 mm) were selected as input factors, whereas feed force, thrust force, cutting force, surface roughness, and specific cutting pressure were considered output responses. Experiments were conducted using a Taguchi L27 orthogonal array (OA). The proposed methodology integrates grey relational analysis (GRA) with fuzzy logic (FL) to obtain a grey-fuzzy reasoning grade (GFRG) for multi-response optimisation. Analysis of variance (ANOVA) was employed to identify the most influential machining parameter. The results demonstrated that the grey-fuzzy approach provided a more discriminative optimisation index than conventional grey relational analysis by reducing uncertainty in multi-response decision-making. The confirmation experiments revealed an increase in GFRG from 0.550 to 0.900, corresponding to a relative improvement of 63.64% at the optimal parameter setting. The proposed methodology demonstrates that integrating grey relational analysis with fuzzy inference provides a reliable and statistically supported approach for multi-response optimisation of dry turning parameters for Incoloy 800H.