Mitigating degradation in high-voltage LiNi 0.5 Mn 1.5 O 4 cathodes via Daniele Callegari, Mauro Coduri, Umberto Anselmi Tamburini, Eliana Quartarone
Micrometre-sized single-crystal LiNi 0.5 Mn 1.5 O 4 , obtained by scalable spray pyrolysis and annealing, delivers over 110 mAh g −1 with 71% capacity retention after 1000 cycles at 1C, while suppressing microcracking and transition-metal dissolution.