Investigating Benzoic Acid Derivatives as Potential Atomic Layer Deposition Inhibitors Using Nanoscale Infrared Spectroscopy

Saumya Satyarthy, Mark Cheng, Ayanjeet Ghosh

Area-selective atomic layer deposition (AS-ALD) is a technique utilized for the fabrication of patterned thin films in the semiconductor industry due to its capability to produce uniform and conformal structures with control over thickness at the atomic scale level. In AS-ALD, surfaces are functionalized such that only specific locations exhibit ALD growth, thus leading to spatial selectivity. Self-assembled monolayers (SAMs) are commonly used as ALD inhibiting agents for AS-ALD. However, the choice of organic molecules as viable options for AS-ALD remains limited and the precise effects of ALD nucleation and exposure to ALD conditions on the structure of SAMs is yet to be fully understood. In this work, we investigate the potential of small molecule carboxylates as ALD inhibitors, namely benzoic acid and two of its derivatives, 4-trifluoromethyl benzoic acid (TBA), and 3,5-Bis (trifluoromethyl)benzoic acid (BTBA) and demonstrate that monolayers of all three molecules are viable options for applications in ALD blocking. We find that the fluorinated SAMs are better ALD inhibitors; however, this property arises not from the hydrophobicity but the coordination chemistry of the SAM. Using nanoscale infrared spectroscopy, we probe the buried monolayer interface to demonstrate that the distribution of carboxylate coordination states and their evolution is correlated with ALD growth, highlighting the importance of the interfacial chemistry in optimizing and assessing ALD inhibitors.

More from our Archive