Fractal Acoustic Emission Characteristics and Energy Evolution of High-Water-Resistance Concrete Backfill: Roles of Water-to-Cement Ratio and Fiber Volume Fraction
Shuaigang Liu, Zizheng Zhang, Jianxiong Yang, Kun Fang, Zilu Liu, Xiaohe WangFiber-reinforced high-water-resistance concrete backfill (FHWCB) is a rapid-setting cementitious backfill system used for underground support and backfilling, but its stability is strongly affected by mixture water content and fiber dispersion. This study investigated the fresh-state behavior, mechanical performance, acoustic emission (AE) fractal characteristics, b-value response, and energy evolution of FHWCB. Mixtures with water-to-cement ratios (w/c) of 1.0–1.8 and fiber volume fractions (Vf) of 0–0.5% were prepared and tested using fresh property measurements, unconfined compression, thermogravimetry, AE monitoring, correlation dimension analysis, b-value analysis, and strain energy partitioning. Increasing w/c improved flowability and delayed setting, but weakened the hydration skeleton and reduced early-age compressive strength by approximately 56–61%. Fiber reinforcement showed a non-monotonic effect: Vf = 0.3% increased compressive strength by approximately 16–26%, whereas excessive fiber addition reduced strength because of fiber clustering and weak local zones. AE amplitude sequences exhibited measurable fractal characteristics. A higher correlation dimension indicated distributed microdamage, while decreasing correlation dimension and b-value reflected the transition toward localized macrocrack growth. Energy analysis showed that the peak elastic strain energy density decreased from approximately 0.60 to 0.39 MJ/m3 as w/c increased. The proposed AE fractal–b-value–energy framework provides a quantitative basis for tracking damage progression and optimizing FHWCB for underground engineering.