Dendrite Structure Refinement and Mechanical Property Improvement of a Single-Crystal Superalloy

Hongyuan Sun, Dexin Ma, Yunxing Zhao, Jianhui Wei, Xiaoyi Gong, Zhongyuan Sun

In the present work, the effect of different casting processes on the microstructure and creep properties of the second-generation single-crystal superalloy DD419 was investigated. Under conventional production conditions and a contour-suited thermal insulation method, single-crystal rods of types A and B were fabricated, respectively. In comparison to rod type A, the solidification process of rod type B featured a 1.6-fold increase in the temperature gradient and a 32% reduction in primary dendrite spacing. The γ/γ′ eutectic in the as-cast microstructure, the residual eutectic phase, and porosity after heat treatment were also significantly reduced, resulting in the improved homogeneity of the single crystal castings. Under the testing conditions of 850 °C/650 MPa and 1050 °C/190 MPa, the stress rupture life of sample B was enhanced by 25% and 5.2%, respectively, compared to sample A. Therefore, due to dendrite structure refinement, the stress rupture life of the superalloy was evidently improved, especially at medium temperatures.

More from our Archive