DOI: 10.1039/d4ra07749k ISSN: 2046-2069

Composition of the isopropanol-soluble portion and fast pyrolysis product distribution of the insoluble part from Pakistani lignite

Gui-han Zhao, Ya-ya Ma, Yuan Ren, Jun Xiao, Wen-Long Mo, Jia Guo, Xian-Yong Wei, Xing Fan, Akram Naeem

Pakistani lignite (PLC) was thermally dissolved at 300 °C using isopropanol (IPA) to obtain a soluble portion (SP) and insoluble portion (ISP).